I used some hydrospan 100 to make a head that i want to enlarge. It came out of the mould fine and the only thing i would have to fix was the tip of the nose and the bubble in the chin.
According to the tutorial, when you demould the head after letting it cure for 24 hours it should be a brownish colour and fairly hard but mine was a light Jade green and slightly squishy.
I thought this was odd but decided to put it in some water anyway and although the head is enlarging, it is flaking apart.
Any suggestions what might have caused this?
The H100 was new and unsealed until i did this head.
According to the tutorial, when you demould the head after letting it cure for 24 hours it should be a brownish colour and fairly hard but mine was a light Jade green and slightly squishy.
I thought this was odd but decided to put it in some water anyway and although the head is enlarging, it is flaking apart.
Any suggestions what might have caused this?
The H100 was new and unsealed until i did this head.
Comment