meant to post this a while back, but I sprayed a zubber made item with flex seal. I only gave it a once over (one coat), and it stuck to the zubber pretty well. I was also able to paint it using testors acrylic. If I bent the toy the flex cracked a little but still stuck. This is why I had mentioned only one coat was applied. Had I done two or three coats it might very well not crack at all. Seeing that Zubber is way more greasy than alumnite it is a safe bet it would be even better on that material
Calling this a finished custom (and now in that sub forum as well). A 1970's style crudely made rubber monster prehistoric shark or thing from the see-- cheers
Last edited by mazinz; Jun 10, '12 at 3:37 PM.
"What motivated him to throw a puppy at the Hells Angels is currently unclear,"